Abstract
Single-pass frequency conversion of 20-picosecond 1.064/1.203 μm Nd:YAG/CaCO3 Raman laser radiation into the wavelength of 9.21 μm with a 10-μJ level of output pulse energy by difference-frequency generation in a LiGaS2 crystal is demonstrated.
© 2019 The Author(s)